Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PUR-Ester Witcobond® W-240 CHEMTURU USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | CHEMTURU USA/Witcobond® W-240 |
---|---|---|---|
Shore hardness | 48.0 | ||
Hardness | F |
Supplementary Information | Test Condition | Test Method | CHEMTURU USA/Witcobond® W-240 |
---|---|---|---|
Cosolvent-N-Methylpyrrolidone | 12 % | ||
Minimum Film Forming Temperature | 0 °C |
thermosetting | Test Condition | Test Method | CHEMTURU USA/Witcobond® W-240 |
---|---|---|---|
Thermosetting mixed viscosity | 25°C | <60.0 cP |
elastomer | Test Condition | Test Method | CHEMTURU USA/Witcobond® W-240 |
---|---|---|---|
elongation | 断裂 | 70 % | |
tensile strength | 41.4 MPa |
physical property | Test Condition | Test Method | CHEMTURU USA/Witcobond® W-240 |
---|---|---|---|
Solid Content | 29to31 % | ||
density | 1.05 g/cm³ | ||
pH value | 25°C | 7.5to9.0 |
Thermal performance | Test Condition | Test Method | CHEMTURU USA/Witcobond® W-240 |
---|---|---|---|
Glass Transition Temperature | -53.0 °C |