Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPEE CM550-S DSM HOLAND
Arnitel®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | DSM HOLAND/CM550-S |
|---|---|---|---|
| Shore hardness | Shore D, 15 Sec | ISO 868 | 57 |
| Shore A, 15 Sec | ISO 868 | 97 | |
| Shore A, 3 Sec | ISO 868 | 98 | |
| Shore D, 3 Sec | ISO 868 | 57 |
| thermal performance | Test Condition | Test Method | DSM HOLAND/CM550-S |
|---|---|---|---|
| Melting temperature | ISO 11357-3 | 205 °C | |
| Vicat softening temperature | ISO 306/B50 | 71.0 °C |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/CM550-S |
|---|---|---|---|
| Nominal tensile fracture strain | ISO 527-2 | 430 % | |
| Tensile modulus | ISO 527-2 | 205 Mpa | |
| tensile strength | 100% Strain | ISO 527-2 | 17.0 Mpa |
| 5.0% Strain | ISO 527-2 | 9.70 Mpa | |
| 50% Strain | ISO 527-2 | 18.0 Mpa | |
| Break | ISO 527-2 | 27.0 Mpa | |
| 10% Strain | ISO 527-2 | 14.0 Mpa |
| Electrical performance | Test Condition | Test Method | DSM HOLAND/CM550-S |
|---|---|---|---|
| Dissipation factor | 100 Hz | IEC 60250 | 0.018 |
| 1 MHz | IEC 60250 | 0.050 | |
| Relative permittivity | 100 Hz | IEC 60250 | 4.20 |
| 1 MHz | IEC 60250 | 3.50 | |
| Volume resistivity | IEC 60093 | > 1.0E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | DSM HOLAND/CM550-S |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 230°C/2.16 kg | ISO 1133 | 17.0 cm3/10min |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.11 % |