Unspecified Rigid Cast RC-8017 BJB Enterprises, Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Supplementary InformationTest ConditionTest MethodBJB Enterprises, Inc./Rigid Cast RC-8017
CureTime25°C5.0to7.0 day
hardnessTest ConditionTest MethodBJB Enterprises, Inc./Rigid Cast RC-8017
Shore hardnessShoreDASTM D224078to82
thermal performanceTest ConditionTest MethodBJB Enterprises, Inc./Rigid Cast RC-8017
Hot deformation temperature1.8MPa,UnannealedASTM D64860.0 °C
0.45MPa,UnannealedASTM D64871.1 °C
mechanical propertiesTest ConditionTest MethodBJB Enterprises, Inc./Rigid Cast RC-8017
Bending modulusASTM D7901520 MPa
bending strengthYieldASTM D79057.0 MPa
elongationYieldASTM D63814 %
Tensile modulusASTM D6381860 MPa
tensile strengthASTM D63846.9 MPa
thermosettingTest ConditionTest MethodBJB Enterprises, Inc./Rigid Cast RC-8017
Thermosetting componentsPartA按重量计算的混合比:100.按容量计算的混合比:100
PartB按重量计算的混合比:88.按容量计算的混合比:100
Thermosetting mixed viscosity43°CBrookfield400 cP
GelTimeBrookfield0.9to1.1 min
WorkTime9Brookfield0.9to1.1 min
25°C6Brookfield1300 cP
43°C7Brookfield350 cP
25°C5Brookfield550 cP
Demold Time8Brookfield40to60 min
25°CBrookfield900 cP
Physical propertiesTest ConditionTest MethodBJB Enterprises, Inc./Rigid Cast RC-8017
density--11.04 g/cm³
--21.19 g/cm³
Shrinkage rate--30.40 %
--40.20 %
impact performanceTest ConditionTest MethodBJB Enterprises, Inc./Rigid Cast RC-8017
Impact strength of cantilever beam gapASTM D25656 J/m