| mechanical properties | Test Condition | Test Method | COVESTRO GERMANY/DP 1080AU |
|---|---|---|---|
| Tensile storage modulus | -20°C | ISO 6721-1 | 170 Mpa |
| tensile strength | 10% Strain, 23°C | DIN 53504 | 1.30 Mpa |
| Wear resistance | 23°C | IOS 1133 | 35.0 mm³ |
| Tensile strain | Break, 23°C | DIN 53504 | 750 % |
| tensile strength | 300% Strain, 23°C | DIN 53504 | 8.00 Mpa |
| Tensile storage modulus | 60°C | ISO 6721-1 | 24.0 Mpa |
| tensile strength | Break, 23°C | DIN 53504 | 35.0 Mpa |
| 100% Strain, 23°C | DIN 53504 | 4.00 Mpa | |
| Tensile storage modulus | 20°C | ISO 6721-1 | 34.0 Mpa |
| hardness | Test Condition | Test Method | COVESTRO GERMANY/DP 1080AU |
| Shore hardness | Shore A, 1 Sec, 23°C | ISO 7619 | 80 |
| elastomer | Test Condition | Test Method | COVESTRO GERMANY/DP 1080AU |
| Permanent compression deformation | 23°C, 72 hr | ISO 815 | 22 % |
| 70°C, 24 hr5 | ISO 815 | 36 % | |
| 70°C, 24 hr6 | ISO 815 | 27 % | |
| Resilience | 23°C | ISO 4662 | 44 % |
| tear strength | 23°C | ISO 34-1 | 56 kN/m |
| injection | Test Condition | Test Method | COVESTRO GERMANY/DP 1080AU |
| Mold temperature | 20 to 40 °C | ||
| drying temperature | < 80 °C | ||
| Processing (melt) temperature | 185 to 200 °C |