PA6 H100MP AdvanSix
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Supplementary InformationTest ConditionTest MethodAdvanSix/ H100MP
PunctureIndex23°C181.5 kN/m
Puncture Resistance23°C960 g
filmTest ConditionTest MethodAdvanSix/ H100MP
GravesTearTD:23°CASTM D10042070 N
tensile strength TD:断裂ASTM D88280.0 MPa
GravesTearMD:23°CASTM D10042140 N
elongationMD:断裂ASTM D882340 %
Carbon dioxide transmittance23°CASTM D14341130 cm³/m²/24hr
Tensile modulusMDASTM D882700 MPa
tensile strength MD:断裂ASTM D88290.0 MPa
Nitrogen transfer rate23°CASTM D1434217 cm³/m²/24hr
Water Vapor Transmission Rate23°CASTMF1249990 g/m²/24hr
Tensile modulusTDASTM D882590 MPa
tensile strength TD:屈服ASTM D88230.0 MPa
OTr23°CASTM D3985620 cm³/m²/24hr
tensile strength MD:屈服ASTM D88230.0 MPa
elongationTD:断裂ASTM D882340 %
physical property Test ConditionTest MethodAdvanSix/ H100MP
water contentASTM D6869<0.080 %
densityASTM D15051.13 g/cm³
Water absorption rate饱和ASTM D5709.5 %
24hrASTM D5701.6 %
平衡ASTM D5702.7 %
melt mass-flow rate235°C/1.0kgASTM D12382.6 g/10min
Thermal performanceTest ConditionTest MethodAdvanSix/ H100MP
melting temperature220 °C