Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PBT T401 Nanjing Hongrui
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Basic performanceTest ConditionTest MethodNanjing Hongrui/T401
densityASTM D-7921.25 g/cm
Mechanical propertiesTest ConditionTest MethodNanjing Hongrui/T401
elongation断裂ASTM D-63830 %
Rockwell hardness110
bending strength屈服ASTM D-79055 MPa
Impact strength of cantilever beam gapASTM D-2505.0 KJ/m
Flexural modulusASTM D-7901500 MPa
tensile strength 断裂ASTM D-63838 MPa
Electrical performanceTest ConditionTest MethodNanjing Hongrui/T401
Surface ResistivityASTM D-25710 Ω
dielectric strengthASTM D-14915 KV/mm
physical property Test ConditionTest MethodNanjing Hongrui/T401
Shrinkage rateASTM D-9550.013-0.024 mm/mm
Thermal performanceTest ConditionTest MethodNanjing Hongrui/T401
Heat distortion temperature0.45MPa,HDTASTM D-648120
melting temperature220-225
UL flame retardant ratingUL 94HB