HDPE PRE-ELEC® PE 1202 Premix Oy
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Premix Oy/PRE-ELEC® PE 1202 |
---|---|---|---|
Charpy Notched Impact Strength | -20°C | ASTM D256 | 23 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO 180 | 43 kJ/m² |
Charpy Notched Impact Strength | 23°C | ASTM D256 | 36 kJ/m² |
Impact strength of cantilever beam gap | -20°C | ISO 180 | 18 kJ/m² |
Suspended wall beam without notch impact strength | -20°C,4.00mm | ASTM D256 | NoBreak |
Impact strength of simply supported beam without notch | 23°C | ASTM D256 | NoBreak |
-20°C | ASTM D256 | NoBreak | |
-20°C | ISO 179 | NoBreak | |
Charpy Notched Impact Strength | 23°C | ISO 179 | 36 kJ/m² |
Suspended wall beam without notch impact strength | -20°C | ISO 180 | NoBreak |
Impact strength of cantilever beam gap | -20°C,4.00mm,Area | ASTM D256 | 16.8 kJ/m² |
23°C,4.00mm,Area | ASTM D256 | 44.1 kJ/m² | |
Impact strength of simply supported beam without notch | 23°C | ISO 179 | NoBreak |
Suspended wall beam without notch impact strength | 23°C | ISO 180 | NoBreak |
Charpy Notched Impact Strength | -20°C | ISO 179 | 24 kJ/m² |
Suspended wall beam without notch impact strength | 23°C,4.00mm | ASTM D256 | NoBreak |
hardness | Test Condition | Test Method | Premix Oy/PRE-ELEC® PE 1202 |
---|---|---|---|
Shore hardness | 邵氏D | ISO 868 | 66 |
邵氏A | ISO 868 | 95 |
Electrical performance | Test Condition | Test Method | Premix Oy/PRE-ELEC® PE 1202 |
---|---|---|---|
Surface Resistivity | IEC 61340-2-3 | <1.0E+5 ohms | |
Volume resistivity | 内部方法 | <1.0E+4 ohms·cm |
Mechanical properties | Test Condition | Test Method | Premix Oy/PRE-ELEC® PE 1202 |
---|---|---|---|
tensile strength | ASTM D638 | 13.1 MPa | |
Tensile strain | 断裂,4.00mm | ISO 527-2 | 30 % |
屈服 | ISO 527-2 | 10 % | |
Flexural modulus | 4.00mm | ASTM D790 | 1200 MPa |
4.00mm | ISO 178 | 1200 MPa | |
tensile strength | 屈服 | ASTM D638 | 26.9 MPa |
屈服 | ISO 527-2 | 31.0 MPa | |
4.00mm | ISO 527-2 | 13.0 MPa |
physical property | Test Condition | Test Method | Premix Oy/PRE-ELEC® PE 1202 |
---|---|---|---|
Shrinkage rate | MD | ASTM D955 | 1.5to2.5 % |
MD | ISO 294-4 | 1.5to2.5 % | |
density | ASTM D792 | 1.08 g/cm³ | |
ISO 1183 | 1.09 g/cm³ | ||
melt mass-flow rate | 190°C/21.6kg | ISO 1133 | 2.0 g/10min |
Thermal performance | Test Condition | Test Method | Premix Oy/PRE-ELEC® PE 1202 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648A | 87.2 °C |
1.8MPa,未退火,HDT | ISO 75-2/Af | 87.0 °C | |
0.45MPa,未退火,HDT | ASTM D648B | 83.9 °C | |
vicat | -- | ISO 306/A50 | 128 °C |
-- | ASTM D15253 | 128 °C | |
-- | ASTM D15254 | 81.1 °C | |
-- | ISO 306/B50 | 81.0 °C | |
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/Bf | 84.0 °C |