Material Comparison
Add Comparison Model
Highlight Differences
Hide Same

Product Name / Manufacturer / Model

Brand

Typical Applications

Properties

Color

Form

Processing Methods

Grade

Filler

Recycled Content

Certificates

Reference Price

mechanical propertiesTest ConditionTest MethodSTYRON TAIWAN/8600 BK
bending strengthISO 17894 MPa
tensile strengthYieldISO 527-260 MPa
Tensile strainBreakISO 527-2100 %
Bending modulusISO 1782400 MPa
tensile strengthBreakISO 527-258 MPa
Rockwell hardnessISO 2039-2123 R
Physical propertiesTest ConditionTest MethodSTYRON TAIWAN/8600 BK
melt mass-flow rateISO 113320 g/10min
densityISO 1183/B1.20
Shrinkage rateISO 294-40.5-0.7 %
thermal performanceTest ConditionTest MethodSTYRON TAIWAN/8600 BK
Vicat softening temperature-ISO 306/A150
Extreme Oxygen IndexISO 4589-235 %
Linear coefficient of thermal expansionASTM D6960.000065 cm/cm/℃
UL flame retardant rating1.5mmUL94V-0
Hot deformation temperature1.8Mpa,UnannealedISO 75-2A122
UL flame retardant rating2.5mmUL945VA
Hot deformation temperature0.45Mpa,UnannealedISO 75-2B136