PC 8600 BK STYRON TAIWAN
EMERGE™
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | STYRON TAIWAN/8600 BK |
|---|---|---|---|
| Extreme Oxygen Index | ISO 4589-2 | 35 % | |
| Hot deformation temperature | 0.45Mpa,Unannealed | ISO 75-2B | 136 ℃ |
| 1.8Mpa,Unannealed | ISO 75-2A | 122 ℃ | |
| Linear coefficient of thermal expansion | ASTM D696 | 0.000065 cm/cm/℃ | |
| UL flame retardant rating | 2.5mm | UL94 | 5VA |
| 1.5mm | UL94 | V-0 | |
| Vicat softening temperature | - | ISO 306/A | 150 ℃ |
| mechanical properties | Test Condition | Test Method | STYRON TAIWAN/8600 BK |
|---|---|---|---|
| Bending modulus | ISO 178 | 2400 MPa | |
| bending strength | ISO 178 | 94 MPa | |
| Rockwell hardness | ISO 2039-2 | 123 R | |
| Tensile strain | Break | ISO 527-2 | 100 % |
| tensile strength | Yield | ISO 527-2 | 60 MPa |
| Break | ISO 527-2 | 58 MPa |
| Physical properties | Test Condition | Test Method | STYRON TAIWAN/8600 BK |
|---|---|---|---|
| density | ISO 1183/B | 1.20 | |
| melt mass-flow rate | ISO 1133 | 20 g/10min | |
| Shrinkage rate | ISO 294-4 | 0.5-0.7 % |