Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP PM970W SUNALLOMER JAPAN
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic Performance | Test Condition | Test Method | SUNALLOMER JAPAN/PM970W |
---|---|---|---|
density | JIS K 6921-2 | 0.9 | |
melt mass-flow rate | JIS K 6921-2 | 30 g/10min |
thermal performance | Test Condition | Test Method | SUNALLOMER JAPAN/PM970W |
---|---|---|---|
Hot deformation temperature | 0.46MPa | JIS K 6921-2 | 93 °C |
mechanical properties | Test Condition | Test Method | SUNALLOMER JAPAN/PM970W |
---|---|---|---|
Bending modulus | JIS K 6921-2 | 1100 Mpa | |
ASTM D790/ISO 178 | 1100(MPa) kg/cm²(MPa)[Lb/in²] | ||
Charpy Notched Impact Strength | -20℃ | JIS K 6921-2 | 2.4 KJ/m |
23℃ | JIS K 6921-2 | 7.1 KJ/m | |
elongation | Break | JIS K 6921-2 | 60 % |
Rockwell hardness | ASTM D785 | 83 | |
JIS K 7202 | 83 HRR | ||
Tensile modulus | ASTM D638/ISO 527 | 1050(MPa) kg/cm²(MPa)[Lb/in²] | |
JIS K 6921-2 | 1050 Mpa | ||
tensile strength | JIS K 6921-2 | 25 Mpa |
Physical properties | Test Condition | Test Method | SUNALLOMER JAPAN/PM970W |
---|---|---|---|
density | ASTM D792/ISO 1183 | 0.9 |
optical performance | Test Condition | Test Method | SUNALLOMER JAPAN/PM970W |
---|---|---|---|
gloss | 60° | JIS Z 8741 | 67 % |