Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
HIPS SEHI-128 IDEMITSU MALASIA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Mechanical propertiesTest ConditionTest MethodIDEMITSU MALASIA/SEHI-128
elongation断裂ASTM D63830 %
tensile strength 断裂ASTM D63826.5 MPa
flammabilityTest ConditionTest MethodIDEMITSU MALASIA/SEHI-128
UL flame retardant rating1.50 mmUL 94V-2
squeeze outTest ConditionTest MethodIDEMITSU MALASIA/SEHI-128
drying temperature70.0 °C
die temperature190 to 220 °C
drying time1.0 to 2.0 hr
Barrel Temperature200 to 240 °C
physical property Test ConditionTest MethodIDEMITSU MALASIA/SEHI-128
densityASTM D7921.11 g/cm³
melt mass-flow rate200°C/5.0 kgASTM D12384.0 g/10 min
injectionTest ConditionTest MethodIDEMITSU MALASIA/SEHI-128
drying time1.0 to 2.0 hr
Temperature in the middle of the barrel190 to 220 °C
Temperature at the rear of the barrel180 to 210 °C
drying temperature70.0 °C
Temperature at the front of the material cylinder210 to 240 °C
Temperature40.0 to 60.0 °C
Spray nozzle temperature200 to 230 °C
Thermal performanceTest ConditionTest MethodIDEMITSU MALASIA/SEHI-128
Heat distortion temperature1.8 MPa, 未退火,HDTASTM D64881.0 °C