| hardness | Test Condition | Test Method | ASAHI JAPAN/CR301 BK |
|---|---|---|---|
| Rockwell hardness | M -Sale | ISO 2039-2 | 85 |
| M-Scale | ASTM D785 | 85 |
| thermal performance | Test Condition | Test Method | ASAHI JAPAN/CR301 BK |
|---|---|---|---|
| Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 191 °C |
| 0.45 MPa, Unannealed | ISO 75-2/B | 249 °C | |
| 1.8 MPa, Unannealed | ISO 75-2/A | 188 °C | |
| 0.45 MPa, Unannealed | ASTM D648 | 250 °C | |
| Linear coefficient of thermal expansion | Flow | ASTM D696 | 4.0E-5 cm/cm/°C |
| mechanical properties | Test Condition | Test Method | ASAHI JAPAN/CR301 BK |
|---|---|---|---|
| Bending modulus | 23°C | ISO 178 | 7400 Mpa |
| -- | ASTM D790 | 5900 Mpa | |
| bending strength | 23°C | ISO 178 | 140 Mpa |
| -- | ASTM D790 | 147 Mpa | |
| elongation | Break, 23°C | ISO 527-2 | 2.0 % |
| Break | ASTM D638 | 3.0 % | |
| Taber abraser | 1000 Cycles | ASTM D1044 | -- mg |
| Tensile modulus | 23°C | ISO 527-2 | 7000 Mpa |
| tensile strength | Break, 23°C | ISO 527-2 | 85.0 Mpa |
| -- | ASTM D638 | 88.0 Mpa |
| Physical properties | Test Condition | Test Method | ASAHI JAPAN/CR301 BK |
|---|---|---|---|
| Shrinkage rate | Flow | Internal Method | 0.50 - 1.3 % |
| Water absorption rate | Saturation, 23°C | -- % | |
| Equilibrium, 23°C, 50% RH | ISO 62 | -- % |
| impact performance | Test Condition | Test Method | ASAHI JAPAN/CR301 BK |
|---|---|---|---|
| Impact strength of simply supported beam without notch | ISO 179 | 51 kJ/m² |
| flammability | Test Condition | Test Method | ASAHI JAPAN/CR301 BK |
|---|---|---|---|
| UL flame retardant rating | 0.75 mm | UL 94 | HB |