Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC AZ1900-V0 BK IDEMITSU JAPAN
TARFLON™
Electrical applications,Casters,Thin walled products
Low viscosity,Flame retardant
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | IDEMITSU JAPAN/AZ1900-V0 BK |
---|---|---|---|
Rockwell hardness | R -Sale | ISO 2039-2 | 120 |
M -Sale | ISO 2039-2 | 50 |
thermal performance | Test Condition | Test Method | IDEMITSU JAPAN/AZ1900-V0 BK |
---|---|---|---|
Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 125 °C |
Linear coefficient of thermal expansion | Flow | ISO 11359-2 | 6.5E-5 cm/cm/°C |
RTI | UL 746 | 80.0 °C | |
RTI Elec | UL 746 | 80.0 °C | |
RTI Imp | UL 746 | 80.0 °C |
mechanical properties | Test Condition | Test Method | IDEMITSU JAPAN/AZ1900-V0 BK |
---|---|---|---|
Bending modulus | ISO 178 | 2300 Mpa | |
bending strength | ISO 178 | 90.0 Mpa | |
Nominal tensile fracture strain | ISO 527-2 | 95 % | |
tensile strength | Yield | ISO 527-2 | 65.0 Mpa |
Electrical performance | Test Condition | Test Method | IDEMITSU JAPAN/AZ1900-V0 BK |
---|---|---|---|
Compared to the anti leakage trace index | UL 746 | PLC 2 | |
Dielectric constant | 1 MHz | IEC 60250 | 2.85 |
Dielectric strength | IEC 60243-1 | 30 KV/mm |
Physical properties | Test Condition | Test Method | IDEMITSU JAPAN/AZ1900-V0 BK |
---|---|---|---|
Melt Volume Flow Rate (MVR) | 300°C/1.2 kg | ISO 1133 | 18.0 cm3/10min |
Shrinkage rate | Flow : 2.00 mm | Internal Method | 0.50 - 0.70 % |
横向Flow : 2.00 mm | Internal Method | 0.50 - 0.70 % | |
Spiral flow length | Internal Method | 29.0 CM | |
Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.23 % |
flammability | Test Condition | Test Method | IDEMITSU JAPAN/AZ1900-V0 BK |
---|---|---|---|
ISO | >PC< | ||
UL flame retardant rating | 1.5 mm | UL 94 | V-0 |
injection | Test Condition | Test Method | IDEMITSU JAPAN/AZ1900-V0 BK |
---|---|---|---|
drying temperature | 120 °C | ||
drying time | 5.0 to 8.0 hr | ||
Mold temperature | 80 to 120 °C | ||
Temperature at the front of the material cylinder | 260 to 300 °C | ||
Temperature at the rear of the barrel | 260 to 300 °C | ||
Temperature in the middle of the barrel | 260 to 300 °C |