Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA610 CM2001 TORAY JAPAN
Amilan®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | TORAY JAPAN/CM2001 |
|---|---|---|---|
| Rockwell hardness | R-Sale,23°C | 116 -- |
| thermal performance | Test Condition | Test Method | TORAY JAPAN/CM2001 |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | °C | 180 -- |
| Linear coefficient of thermal expansion | MD | cm/cm/°C | 1.2E-04 -- |
| Melting temperature | °C | 225 -- | |
| specific heat | J/kg/°C | 1900 -- | |
| thermal conductivity | W/m/K | 0.25 -- |
| mechanical properties | Test Condition | Test Method | TORAY JAPAN/CM2001 |
|---|---|---|---|
| Bending modulus | 23°C | MPa | 2000 900 |
| -40°C | MPa | 2300 -- | |
| 80°C | MPa | 500 -- | |
| bending strength | 23°C | MPa | 95.0 55.0 |
| Compressive stress | 23°C | MPa | 65.0 -- |
| shear strength | 23°C | MPa | 50.0 45.0 |
| Taber abraser | 1000Cycles | mg | 4.00 -- |
| Tensile strain | Break,23°C | % | 50 |
| tensile strength | -40°C | MPa | 85.0 -- |
| 80°C | MPa | 25.0 -- | |
| 23°C | MPa | 55.0 40.0 |
| Electrical performance | Test Condition | Test Method | TORAY JAPAN/CM2001 |
|---|---|---|---|
| Dielectric constant | 23°C,50Hz | 3.90 -- | |
| 23°C,1kHz | 3.60 -- | ||
| 23°C,1MHz | 3.10 -- | ||
| Dissipation factor | 23°C,1MHz | 0.020 -- | |
| 23°C,50Hz | 0.040 -- | ||
| 23°C,1kHz | 0.040 -- | ||
| Volume resistivity | ohms·cm | 1.0E+13-1.0E+14 -- |
| Physical properties | Test Condition | Test Method | TORAY JAPAN/CM2001 |
|---|---|---|---|
| Shrinkage rate | MD:1.00mm2 | % | 0.30-0.70 -- |
| MD:3.00mm3 | % | 0.70-1.3 -- | |
| Water absorption rate | Saturation,23°C | % | 4.0 -- |
| 23°C,24hr | % | 0.30 -- |
| impact performance | Test Condition | Test Method | TORAY JAPAN/CM2001 |
|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | 无断裂 |