NBR NANCAR® 1203LD Nantex Industry Co., Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | Nantex Industry Co., Ltd./NANCAR® 1203LD |
---|---|---|---|
ozone resistance | nocrack |
hardness | Test Condition | Test Method | Nantex Industry Co., Ltd./NANCAR® 1203LD |
---|---|---|---|
Shore hardness | 邵氏A | 72 |
physical property | Test Condition | Test Method | Nantex Industry Co., Ltd./NANCAR® 1203LD |
---|---|---|---|
bound acrylonitrile content | 内部方法 | 28.0 % | |
Mooney viscosity | ML1+4,100°C | ASTM D1646 | 66 MU |
elastomer | Test Condition | Test Method | Nantex Industry Co., Ltd./NANCAR® 1203LD |
---|---|---|---|
tensile strength | 屈服 | 12.7 MPa | |
compression set | 100°C | 45 % | |
elongation | 断裂 | 370 % |
aging | Test Condition | Test Method | Nantex Industry Co., Ltd./NANCAR® 1203LD |
---|---|---|---|
Change rate of hardness (Shore) in the air | 支撐A,100°C,70hr,在IRM903油中 | 2.0 | |
volume change | 100°C,70hr,在IRM903油中 | 2.0 % | |
Change rate of ultimate elongation in air | 100°C,70hr,在IRM903油中 | -32 % | |
100°C,70hr | -38 % | ||
100°C,70hr,在ASTM#1油中 | -43 % | ||
Change rate of tensile strength in air | 100°C,70hr | 3.0 % | |
100°C,70hr,在ASTM#1油中 | 14 % | ||
Change rate of hardness (Shore) in the air | 支撐A,100°C,70hr,在ASTM#1油中 | 10 | |
Change rate of tensile strength in air | 100°C,70hr,在IRM903油中 | 12 % | |
Change rate of hardness (Shore) in the air | 100°C,70hr | 2.0 | |
volume change | 100°C,70hr,ASTM标准油(1号) | -12 % |
Thermal performance | Test Condition | Test Method | Nantex Industry Co., Ltd./NANCAR® 1203LD |
---|---|---|---|
Heat loss | ASTM D5688 | 0.30 % |