ABS+PMMA (0.160 inch) Aristech Acrylics LLC
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodAristech Acrylics LLC/(0.160 inch)
Impact strength of cantilever beam gap4.10mmASTM D256A110 J/m
Dart impact4.10mm内部方法16.7 J
hardnessTest ConditionTest MethodAristech Acrylics LLC/(0.160 inch)
Rockwell hardnessM级,4.10mmASTM D78567
Barcol Hardness4.10mmASTM D258354
Supplementary InformationTest ConditionTest MethodAristech Acrylics LLC/(0.160 inch)
HotFormingTemperatureABSSide:4.10mm内部方法149to171 °C
AcrylicSide:4.10mm内部方法177to193 °C
Odor(4.10mm)内部方法None
Mechanical propertiesTest ConditionTest MethodAristech Acrylics LLC/(0.160 inch)
Tensile modulus4.10mmASTM D6382550 MPa
Flexural modulus4.10mm4ASTM D7902250 MPa
elongation断裂,4.10mmASTM D6384.4 %
bending strength4.10mm4ASTM D79074.5 MPa
tensile strength 屈服,4.10mmASTM D63845.5 MPa
bending strength4.10mm3ASTM D79062.7 MPa
Flexural modulus4.10mm3ASTM D7902340 MPa
optical performance Test ConditionTest MethodAristech Acrylics LLC/(0.160 inch)
gloss60°,4.10µmASTM D52387
physical property Test ConditionTest MethodAristech Acrylics LLC/(0.160 inch)
Water absorption rate饱和,4.10mmASTM D5700.19 %
densityASTM D7921.09 g/cm³
Thermal performanceTest ConditionTest MethodAristech Acrylics LLC/(0.160 inch)
Heat distortion temperature1.8MPa,未退火,4.10mm,HDTASTM D64885.6 °C
Linear coefficient of thermal expansionMD:4.10mmASTM D6968.5E-05 cm/cm/°C