Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| machinability | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/EHR3400 |
|---|---|---|---|
| Dry conditions | 热风干燥 120℃---約4-8小时 | ||
| Mold temperature | 70-100 °C | ||
| Processing temperature | 240-260 °C | ||
| Screw speed | 50-100 rpm | ||
| mechanical properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/EHR3400 |
| Tensile modulus | ASTM D638/ISO 527 | 2800 kg/cm²(MPa)[Lb/in²] | |
| Elongation at Break | ASTM D638/ISO 527 | 61 % | |
| Bending modulus | ASTM D790/ISO 178 | 2600 kg/cm²(MPa)[Lb/in²] | |
| bending strength | ASTM D790/ISO 178 | 93 kg/cm²(MPa)[Lb/in²] | |
| Physical properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/EHR3400 |
| Shrinkage rate | ASTM D955 | 0.4 - 0.6 % | |
| density | ASTM D792/ISO 1183 | 1.30 | |
| thermal performance | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/EHR3400 |
| Combustibility (rate) | UL 94 | V-0(1.0mm) | |
| Electrical performance | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/EHR3400 |
| Surface resistivity | ASTM D257/IEC 60093 | 6E+15 Ω | |
| Volume resistivity | ASTM D257/IEC 60093 | 3E+14 Ω.cm |