Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC CF-1050 Samsung Cheil South Korea
INFINO®
Phone、Electronic field、Electrical field
High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | Samsung Cheil South Korea/CF-1050 |
---|---|---|---|
Rockwell hardness | R 计秤 | ISO 2039-2 | 120 |
R 级 | ASTM D785 | 120 |
Mechanical properties | Test Condition | Test Method | Samsung Cheil South Korea/CF-1050 |
---|---|---|---|
tensile strength | 屈服 | ISO 527-2/50 | 55.0 Mpa |
屈服3 | ASTM D638 | 59.0 Mpa | |
elongation | 断裂3 | ASTM D638 | 110 % |
bending strength | --4 | ASTM D790 | 83.0 Mpa |
--5 | ISO 178 | 84.0 Mpa | |
Tensile modulus | --3 | ASTM D638 | 2000 Mpa |
-- | ISO 527-2/50 | 2000 Mpa | |
elongation | 断裂 | ISO 527-2/50 | 110 % |
Flexural modulus | --4 | ASTM D790 | 2000 Mpa |
--5 | ISO 178 | 2100 Mpa | |
tensile strength | 断裂3 | ASTM D638 | 59.0 Mpa |
断裂 | ISO 527-2/50 | 69.0 Mpa |
flammability | Test Condition | Test Method | Samsung Cheil South Korea/CF-1050 |
---|---|---|---|
UL flame retardant rating | 2.5 mm | UL 94 | V-2 |
3.0 mm | UL 94 | V-2 | |
0.8 mm | UL 94 | V-2 |
physical property | Test Condition | Test Method | Samsung Cheil South Korea/CF-1050 |
---|---|---|---|
Shrinkage rate | 横向流动 : 3.20 mm | ASTM D955 | 0.40 - 0.70 % |
流量 : 2.00 mm | ISO 294-4 | 0.40 - 0.70 % | |
流动 : 3.20 mm | ASTM D955 | 0.40 - 0.70 % | |
横向流量 : 2.00 mm | ISO 294-4 | 0.40 - 0.70 % | |
melt mass-flow rate | 250°C/10.0 kg | ASTM D1238 | 18 g/10 min |
Thermal performance | Test Condition | Test Method | Samsung Cheil South Korea/CF-1050 |
---|---|---|---|
vicat | -- | ISO 306/B120 | 145 °C |
Heat distortion temperature | 0.45 MPa, 退火, 4.00 mm,HDT | ISO 75-2/B | 136 °C |
vicat | -- | ISO 306/B50 | 141 °C |
Heat distortion temperature | 1.8 MPa, 未退火, 4.00 mm,HDT | ISO 75-2/A | 121 °C |
0.45 MPa, 未退火, 4.00 mm,HDT | ISO 75-2/B | 136 °C | |
1.8 MPa, 退火, 4.00 mm,HDT | ISO 75-2/A | 125 °C |
injection | Test Condition | Test Method | Samsung Cheil South Korea/CF-1050 |
---|---|---|---|
screw speed | 50 to 150 rpm | ||
Suggested maximum moisture content | < 0.050 % | ||
Vacuum dryer | 100 °C | ||
Injection Pressure | 49.0 to 245 Mpa | ||
Hot air dryer | 2.0 to 4.0 hr | ||
Temperature in the middle of the barrel | 260 to 270 °C | ||
Temperature at the rear of the barrel | 240 to 250 °C | ||
Vacuum dryer | 2.0 to 6.0 hr | ||
Temperature at the front of the material cylinder | 280 to 310 °C | ||
Back pressure | 0.490 to 1.96 Mpa | ||
Temperature | 40 to 100 °C | ||
Hot air dryer | 100 °C | ||
Spray nozzle temperature | 290 to 310 °C |