PA6 B 40 EM2 POLIBLEND ITALY
POLIMID B
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | POLIBLEND ITALY/B 40 EM2 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 14 kJ/m² |
Tensile modulus | 23°C | ISO 527-2 | 2500 Mpa |
elongation at break | 23°C | ISO 527-2 | 90 % |
Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | NB kJ/m² |
tensile strength | 23°C | ISO 527-2 | 75 Mpa |
Electrical performance | Test Condition | Test Method | POLIBLEND ITALY/B 40 EM2 |
---|---|---|---|
Dissipation Factor | 相对漏电起痕指数 | IEC 60112 | >600 V |
Volume resistivity | IEC 60093 | 1E+14 Ω.cm |
Flame retardant performance | Test Condition | Test Method | POLIBLEND ITALY/B 40 EM2 |
---|---|---|---|
UL flame retardant rating | UL -94 | HB 0.80mm | |
UL -94 | HB 1.50mm | ||
UL -94 | HB 3.00mm |
physical property | Test Condition | Test Method | POLIBLEND ITALY/B 40 EM2 |
---|---|---|---|
Water absorption rate | (23°C,24hr) | ISO 62 | 1.6/8.5 % |
Shrinkage rate | TD | ISO 294-4 | 1.5 % |
MD | ISO 294-4 | 1.1 % |
Thermal performance | Test Condition | Test Method | POLIBLEND ITALY/B 40 EM2 |
---|---|---|---|
Heat distortion temperature | 1.80MPa退火,HDT | ISO 75-2/Af | 70 °C |
vicat | 熔融温度 | ISO 11357-3 | 222 °C |
Heat distortion temperature | 0.45MPa未退火,HDT | ISO 75-2/Bf | 170 °C |
Linear coefficient of thermal expansion | 耐热/球压测试 | IEC 60695-10-2 | >165 °C |
长期使用温度 | 80 °C | ||
vicat | B9.8N | ISO 306/B50 | 200 °C |