Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPO(PPE)+TPE NORYL™ WCD801AU resin SABIC
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | SABIC/NORYL™ WCD801AU resin |
---|---|---|---|
Shore hardness | 邵氏A,30秒 | ASTM D2240 | 82 |
Electrical performance | Test Condition | Test Method | SABIC/NORYL™ WCD801AU resin |
---|---|---|---|
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | PLC 0 | |
Volume resistivity | ASTM D257 | 2.7E+15 ohms·cm | |
Dissipation Factor | 1MHz | ASTM D150 | 4E-03 |
dielectric constant | 1MHz | ASTM D150 | 2.90 |
dielectric strength | 2.00mm,在油中 | IEC 60243-1 | 20 kV/mm |
Mechanical properties | Test Condition | Test Method | SABIC/NORYL™ WCD801AU resin |
---|---|---|---|
fracture | ISO 527-2/50 | 13.0 MPa | |
ISO 527-2/50 | 110 % | ||
ASTM D638 | 160 % | ||
ASTM D638 | 15.0 MPa | ||
UL 1581 | 21.0 MPa | ||
UL 1581 | 210 % |
flammability | Test Condition | Test Method | SABIC/NORYL™ WCD801AU resin |
---|---|---|---|
Smoke density | Non-Flame,0.5mmplaque,Ds,max | ASTME662 | 130 |
VW | UL 1581 | Pass | |
Hot filament ignition temperature | 3.00mm | IEC 60695-2-13 | 750 °C |
Burning wire flammability index | 3.00mm | IEC 60695-2-12 | 850 °C |
Smoke density | Flame,0.5mmplaque,Ds,max | ASTME662 | 130 |
Limiting Oxygen Index | ISO 4589-2 | 25 % |
physical property | Test Condition | Test Method | SABIC/NORYL™ WCD801AU resin |
---|---|---|---|
density | ASTM D792 | 1.09to1.17 g/cm³ | |
melt mass-flow rate | 250°C/5.0kg | ASTM D1238 | 20 g/10min |
Thermal performance | Test Condition | Test Method | SABIC/NORYL™ WCD801AU resin |
---|---|---|---|
Heat distortion temperature | 100°C | UL 1581 | 15 % |
UL temperature rating | UL 1581 | 80 °C | |
brittle temperature | ASTM D746 | <-40.0 °C |