Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPS A400 F1 TORAY JAPAN
Torelina®
Electrical applications、Casters
Glass fiber reinforced、Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | TORAY JAPAN/A400 F1 |
---|---|---|---|
Water absorption rate | ASTM D-570 | 0.02 % |
Mechanical properties | Test Condition | Test Method | TORAY JAPAN/A400 F1 |
---|---|---|---|
Impact strength of cantilever beam gap | 缺口23℃ | ASTM D-256 | 100 J/m |
Shore hardness | ASTM D-785 | 122 洛氏 | |
tensile strength | ASTM D-638 | 1.3 % | |
coefficient of friction | 对钢 | ASTM D-1894 | 0.28 |
elongation at break | ASTM D-732 | 65 | |
Impact strength of cantilever beam gap | 无缺口23℃ | ASTM D-256 | 25 KJ/m |
bending strength | ASTM D-790 | 190 Mpa | |
abrasion | ASTM D-1044 | 70 mg/1000回 | |
tensile strength | ASTM D-638 | 145 Mpa | |
limiting pv value | 东丽法 | 815 KJ/m | |
bending strength | ASTM D-790 | 15.1 GPa |
Electrical performance | Test Condition | Test Method | TORAY JAPAN/A400 F1 |
---|---|---|---|
dielectric strength | ASTM D-149 | 15 MV/m | |
Induced positive connection | 10 | ASTM D-150 | 0.002 |
Inherent resistance of volume | ASTM D-257 | 10 Ω.m | |
arc resistance | W电极 | ASTM D-495 | 128 秒 |
dielectric constant | 10 | ASTM D-150 | 5.0 |
physical property | Test Condition | Test Method | TORAY JAPAN/A400 F1 |
---|---|---|---|
320℃,98MPa,1mm厚,流动长 | 东丽法 | 110 ×10 | |
Shrinkage rate | 流动方向 | 东丽法 | 0.15 % |
density | ASTM D-792 | 1.90 | |
Shrinkage rate | 垂重方向 | 东丽法 | 0.55 % |
Thermal performance | Test Condition | Test Method | TORAY JAPAN/A400 F1 |
---|---|---|---|
Heat distortion temperature | 1.82MPa,HDT | ASTM D-648 | >260 °C |
combustibility | UL -94 | V-0 | |
Linear coefficient of thermal expansion | 流动方向 | ASTM D-696 | 1.7 ×10 |
melting temperature | DSC | 278 °C | |
Linear coefficient of thermal expansion | 垂重方向 | ASTM D-696 | 2.5 ×10 |
Contact Us
Get App
Top