PP Copolymer 25C21120 4Plas
--
--
Filler, talc filler, 20%, filler by weight,
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | 4Plas/ 25C21120 |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 120 °C |
| Melting temperature | ISO 11357 | 165 °C |
| mechanical properties | Test Condition | Test Method | 4Plas/ 25C21120 |
|---|---|---|---|
| Bending modulus | 23°C | ISO 178 | 2.30 MPa |
| Tensile modulus | 23°C | ISO 527-2/5 | 2000 MPa |
| Tensile strain | Break,23°C | ISO 527-2/5 | 14 % |
| Yield,23°C | ISO 527-2/5 | 5.5 % | |
| tensile strength | Yield,23°C | ISO 527-2/5 | 30.0 MPa |
| Break,23°C | ISO 527-2/5 | 23.0 MPa |
| Physical properties | Test Condition | Test Method | 4Plas/ 25C21120 |
|---|---|---|---|
| density | ISO 1183 | 1.04 g/cm³ | |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 15 g/10min |
| impact performance | Test Condition | Test Method | 4Plas/ 25C21120 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 0.50 kJ/m² |
| -30°C | ISO 179/1eA | 0.30 kJ/m² | |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 4.0 kJ/m² |
| flammability | Test Condition | Test Method | 4Plas/ 25C21120 |
|---|---|---|---|
| Hot filament ignition temperature | 2.0mm | IEC 60695-2-13 | 650 °C |
| UL flame retardant rating | 1.6mm | UL 94 | HB |