| Physical properties | Test Condition | Test Method | TORAY JAPAN/U121 |
|---|---|---|---|
| Water absorption rate | ASTM D570/ISO 62 | 1.7 % | |
| 23°C,24hr | % | 1.7 -- | |
| Shrinkage rate | TD3:3.00mm | % | 1.2-1.3 -- |
| Water absorption rate | Saturation,23°C | % | 8.0 -- |
| density | ASTM D792/ISO 1183 | 1.09 | |
| mechanical properties | Test Condition | Test Method | TORAY JAPAN/U121 |
| bending strength | -40°C | 115 MPa | |
| 23°C | MPa | 80.0 35.0 | |
| ASTM D790/ISO 178 | 115 kg/cm²(MPa)[Lb/in²] | ||
| Tensile strain | Break,23°C | % | 50 |
| Bending modulus | -40°C | MPa | 2500 2500 |
| Elongation at Break | ASTM D638/ISO 527 | 200< % | |
| tensile strength | -40°C | MPa | 90.0 70.0 |
| Tensile strain | Break,-40°C | % | 13 |
| Impact strength of cantilever beam gap | ASTM D256/ISO 179 | 180 kg·cm/cm(J/M)ft·lb/in | |
| tensile strength | 23°C | MPa | 60.0 35.0 |
| Rockwell hardness | ASTM D785 | 114 | |
| Bending modulus | 23°C | 2000 MPa | |
| tensile strength | ASTM D638/ISO 527 | 90 kg/cm²(MPa)[Lb/in²] | |
| Bending modulus | ASTM D790/ISO 178 | 2.5 kg/cm²(MPa)[Lb/in²] | |
| Taber abraser | 1000Cycles | mg | 6.00to7.00 -- |
| thermal performance | Test Condition | Test Method | TORAY JAPAN/U121 |
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 160 ℃(℉) |
| Melting temperature | °C | 225 -- | |
| Hot deformation temperature | 0.45MPa,Unannealed | °C | 160 -- |
| Linear coefficient of thermal expansion | MD | cm/cm/°C | 9.0E-5到1.0E-4 -- |
| Hot deformation temperature | 1.8MPa,Unannealed | °C | 57.0 -- |
| Melting temperature | 225 ℃(℉) | ||
| hardness | Test Condition | Test Method | TORAY JAPAN/U121 |
| Rockwell hardness | R-Sale,23°C | 114 -- |