POE C1055D SABIC INNOVATIVE SAUDI
SABIC® FORTIFY™  
Wire and cable,Footwear
Low Specific Gravity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | SABIC INNOVATIVE SAUDI/C1055D | 
|---|---|---|---|
| Shore hardness | Shore A, 1 Sec | ASTM D2240 | 55 | 
| Shore D, 1 Sec | ASTM D2240 | 12 | 
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE SAUDI/C1055D | 
|---|---|---|---|
| Glass transition temperature | Internal Method | -59.0 °C | |
| Melting temperature | Internal Method | 37.0 °C | 
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE SAUDI/C1055D | 
|---|---|---|---|
| Bending modulus | % Secant | ASTM D790A | 4.40 Mpa | 
| elongation | Yield, Compression Molded | ASTM D638 | > 1000 % | 
| Tensile modulus | Compression Molded,100% Secant | ASTM D638 | 1.40 Mpa | 
| tensile strength | Break, Compression Molded | ASTM D638 | 3.10 Mpa | 
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE SAUDI/C1055D | 
|---|---|---|---|
| melt mass-flow rate | 230°C/2.16 kg | ASTM D1238 | 2.2 g/10 min | 
| 190°C/2.16 kg | ASTM D1238 | 1.0 g/10 min | |
| Mooney viscosity | ML 1+4, 121°C | ASTM D1646 | 24 MU | 
| elastomer | Test Condition | Test Method | SABIC INNOVATIVE SAUDI/C1055D | 
|---|---|---|---|
| tear strength | ASTM D624 | 27.5 kN/m |