Unspecified S&E Wire & Cable GA-1042LF S&E Polymer Solutions, Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | S&E Polymer Solutions, Inc./S&E Wire & Cable GA-1042LF |
---|---|---|---|
Shore hardness | 邵氏A,3秒 | ASTM D2240 | 87to93 |
邵氏A | ASTM D2240 | 94 |
flammability | Test Condition | Test Method | S&E Polymer Solutions, Inc./S&E Wire & Cable GA-1042LF |
---|---|---|---|
Limiting Oxygen Index | ASTM D2863 | 26 % |
elastomer | Test Condition | Test Method | S&E Polymer Solutions, Inc./S&E Wire & Cable GA-1042LF |
---|---|---|---|
elongation | 断裂 | ASTM D412 | 310 % |
tensile strength | 屈服 | ASTM D412 | 18.3 MPa |
100%应变 | ASTM D412 | 11.7 MPa |
physical property | Test Condition | Test Method | S&E Polymer Solutions, Inc./S&E Wire & Cable GA-1042LF |
---|---|---|---|
density | ASTM D792 | 1.32to1.38 g/cm³ |
aging | Test Condition | Test Method | S&E Polymer Solutions, Inc./S&E Wire & Cable GA-1042LF |
---|---|---|---|
Change rate of ultimate elongation in air | 136°C,168hr | UL Unspecified | -19 % |
Change rate of tensile strength in air | 136°C,168hr | UL Unspecified | 10 % |
Thermal performance | Test Condition | Test Method | S&E Polymer Solutions, Inc./S&E Wire & Cable GA-1042LF |
---|---|---|---|
brittle temperature | ASTM D746 | -18.0 °C |