Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PVC Trovidur® ESV R?chling Engineering Plastics SE & Co. KG
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | R?chling Engineering Plastics SE & Co. KG/Trovidur® ESV |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | 8.0 kJ/m² |
Electrical performance | Test Condition | Test Method | R?chling Engineering Plastics SE & Co. KG/Trovidur® ESV |
---|---|---|---|
Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm | |
dielectric constant | IEC 60250 | 3.20 | |
Surface Resistivity | IEC 60093 | >1.0E+13 ohms | |
Dissipation Factor | 1MHz | IEC 60250 | 0.020 |
Mechanical properties | Test Condition | Test Method | R?chling Engineering Plastics SE & Co. KG/Trovidur® ESV |
---|---|---|---|
Tensile modulus | ISO 527-2 | 2500 MPa | |
Tensile strain | 断裂 | ISO 527-2 | 20 % |
physical property | Test Condition | Test Method | R?chling Engineering Plastics SE & Co. KG/Trovidur® ESV |
---|---|---|---|
Water absorption rate | 平衡,23°C,50%RH | ISO 62 | <3.0 % |
density | ISO 1183 | 1.41 g/cm³ |
Thermal performance | Test Condition | Test Method | R?chling Engineering Plastics SE & Co. KG/Trovidur® ESV |
---|---|---|---|
thermal conductivity | DIN 52612 | 0.16 W/m/K | |
Linear coefficient of thermal expansion | MD | DIN 53752 | 6.0E-5到8.0E-5 cm/cm/°C |
Heat distortion temperature | VicatB,HDT | ISO 306 | 74 °C |