mechanical propertiesTest ConditionTest MethodSTYRON TAIWAN/8600-20 IC7700178
tensile strengthYield,4.00mm,InjectionMoldedISO 527-2/5060.0 Mpa
Bending modulus4.00mm,InjectionMoldedISO 1782400 Mpa
Tensile strainYield,4.00mm,InjectionMoldedISO 527-2/506.0 %
tensile strengthBreak,4.00mm,InjectionISO 527-2/5058.0 Mpa
bending strength4.00mm,InjectionMoldedISO 17894.0 Mpa
Tensile strainBreak,4.00mm,InjectionISO 527-2/50100 %
thermal performanceTest ConditionTest MethodSTYRON TAIWAN/8600-20 IC7700178
RTI StrUL 746125 °C
Ball pressure temperatureIEC 60335-1>125 °C
Vicat softening temperature--ISO 306/B50143 °C
--ISO 306/A120150 °C
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B136 °C
RTI ElecUL 746125 °C
RTI ImpUL 746125 °C
Linear coefficient of thermal expansionMD:-40to82°CASTM D6966.5E-05 cm/cm/°C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A122 °C
Physical propertiesTest ConditionTest MethodSTYRON TAIWAN/8600-20 IC7700178
Shrinkage rateISO 294-40.50-0.70 %
melt mass-flow rate300°C/1.2kgISO 113320 g/10min
flammabilityTest ConditionTest MethodSTYRON TAIWAN/8600-20 IC7700178
Ignition temperature of heating wire1.0mmIEC 60695-2-13960 °C
Extreme Oxygen IndexISO 4589-235 %
UL flame retardant rating1.5mmUL 94V-0
hardnessTest ConditionTest MethodSTYRON TAIWAN/8600-20 IC7700178
Rockwell hardnessR-Scale,4.00mmISO 2039-2123