Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PBT VB-5300GS Samsung Cheil South Korea
INFINO®
Electronic and Electrical Applications
enhance,Flame retardant,Filler: Glass fiber reinf
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Samsung Cheil South Korea/VB-5300GS |
|---|---|---|---|
| Rockwell hardness | R-Scale | ASTM D785 | 120 |
| R-Scale | ISO 2039-2 | 117 |
| thermal performance | Test Condition | Test Method | Samsung Cheil South Korea/VB-5300GS |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed,4.00mm | ISO 75-2/A | 207 °C |
| 1.8MPa,Unannealed,6.40mm | ASTM D648 | 210 °C | |
| 0.45MPa,Unannealed,4.00mm | ISO 75-2/B | 222 °C | |
| 0.45MPa,Unannealed,6.40mm | ASTM D648 | 223 °C | |
| Vicat softening temperature | -- | ISO 306/B120 | 212 °C |
| -- | ISO 306/B50 | 210 °C |
| mechanical properties | Test Condition | Test Method | Samsung Cheil South Korea/VB-5300GS |
|---|---|---|---|
| Bending modulus | ISO 178 | 9000 Mpa | |
| ASTM D790 | 9610 Mpa | ||
| bending strength | ASTM D790 | 196 Mpa | |
| ISO 178 | 200 Mpa | ||
| elongation | Break | ASTM D638 | 3.4 % |
| Tensile modulus | ASTM D638 | 7650 Mpa | |
| ISO 527-2/50 | 8000 Mpa | ||
| Tensile strain | Break | ISO 527-2/50 | 3.6 % |
| tensile strength | Yield | ASTM D638 | 127 Mpa |
| Yield | ISO 527-2/50 | 147 Mpa | |
| Break | ASTM D638 | 127 Mpa | |
| Break | ISO 527-2/50 | 150 Mpa |
| Physical properties | Test Condition | Test Method | Samsung Cheil South Korea/VB-5300GS |
|---|---|---|---|
| ash content | ISO 3451 | 30 % | |
| density | ISO 1183 | 1.64 g/cm³ | |
| ASTM D792 | 1.62 g/cm³ | ||
| melt mass-flow rate | 250°C/2.16kg | ISO 1133 | 13 g/10min |
| 250°C/2.16kg | ASTM D1238 | 15 g/10min | |
| Shrinkage rate | MD:3.20mm | ASTM D955 | 0.30-0.90 % |
| Water absorption rate | Equilibrium,23°C | ASTM D570 | 0.060 % |
| impact performance | Test Condition | Test Method | Samsung Cheil South Korea/VB-5300GS |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.7 kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 8.3 kJ/m² |
| 23°C,6.35mm | ASTM D256 | 58 J/m | |
| 23°C,3.18mm | ASTM D256 | 74 J/m |
| flammability | Test Condition | Test Method | Samsung Cheil South Korea/VB-5300GS |
|---|---|---|---|
| UL flame retardant rating | 0.75mm | UL 94 | V-0 |
| 3.0mm | UL 94 | V-0 | |
| 1.7mm | UL 94 | V-0 |