Material Comparison
Add Comparison Model
Highlight Differences
Hide Same

Product Name / Manufacturer / Model

Brand

Typical Applications

Properties

Color

Form

Processing Methods

Grade

Filler

Recycled Content

Certificates

Reference Price

machinabilityTest ConditionTest MethodEXXONMOBIL SAUDI/HYA-600
Dry conditions90
Mold temperature210 °C
Processing temperature220 °C
Melt Temperature190 °C
mechanical propertiesTest ConditionTest MethodEXXONMOBIL SAUDI/HYA-600
Tensile modulusASTM D638/ISO 5271500 kg/cm²(MPa)[Lb/in²]
Elongation at BreakASTM D638/ISO 527450 %
elongationASTM D638/ISO 527500 %
Rockwell hardnessASTM D78562
tensile strengthASTM D638/ISO 52727 kg/cm²(MPa)[Lb/in²]
Physical propertiesTest ConditionTest MethodEXXONMOBIL SAUDI/HYA-600
Water absorption rateASTM D570/ISO 620.002 %
Shrinkage rateASTM D9553.5 %
melt mass-flow rateASTM D1238/ISO 113329 g/10min
densityASTM D792/ISO 11830.954
thermal performanceTest ConditionTest MethodEXXONMOBIL SAUDI/HYA-600
Hot deformation temperatureHDTASTM D648/ISO 75102 ℃(℉)
otherTest ConditionTest MethodEXXONMOBIL SAUDI/HYA-600
purpose家庭.工业和化学品用瓶子.不超过30公升的容器
characteristic吹塑 

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China