TPU 58245 LUBRIZOL USA
ESTANE®
film,Blow molding applications,Blow film,cast film ,Fabric
High elasticity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | LUBRIZOL USA/58245 |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 80 |
| thermal performance | Test Condition | Test Method | LUBRIZOL USA/58245 |
|---|---|---|---|
| Glass transition temperature | ASTM D3418 | -37.0 °C | |
| Kofler Melting Temperature | Internal Method | 135 °C | |
| Melting temperature | DSC | 135 °C |
| film | Test Condition | Test Method | LUBRIZOL USA/58245 |
|---|---|---|---|
| Water vapor permeability | ASTME96 | 1000 g/m²/24hr | |
| 38°C,Mocon法 | ASTM D6701 | 6600 g/m²/24hr |
| mechanical properties | Test Condition | Test Method | LUBRIZOL USA/58245 |
|---|---|---|---|
| Taber abraser | 1000Cycles,1000g,H-18Wheel | ASTM D3389 | 60.0 mg |
| elastomer | Test Condition | Test Method | LUBRIZOL USA/58245 |
|---|---|---|---|
| elongation | Break,0.762mm | ASTM D412 | 700 % |
| Stretch permanent deformation | 200%Strain | ASTM D412 | 10 % |
| tear strength | Split | ASTM D470 | 18 kN/m |
| 0.762mm5 | ASTM D624 | 61.8 kN/m | |
| tensile strength | 300%Strain,0.762mm | ASTM D412 | 8.30 Mpa |
| 100%Strain,0.762mm | ASTM D412 | 4.50 Mpa | |
| Break,0.762mm | ASTM D412 | 31.0 Mpa |