| Physical properties | Test Condition | Test Method | DUPONT USA/FN727 |
|---|---|---|---|
| ThermalConductivityofMelt | 0.16 W/m/K | ||
| MediumDensity | 0.870 g/cm³ | ||
| Shrinkage rate | MD | ISO 294-4 | 0.80 % |
| SpecificHeatCapacity of Melt | 2700 J/kg/°C | ||
| Shrinkage rate | TD | ISO 294-4 | 1.2 % |
| Water absorption rate | Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 1.4 % |
| mechanical properties | Test Condition | Test Method | DUPONT USA/FN727 |
| tensile strength | 50%Strain | ISO 527-2 | 28.0 Mpa |
| Tensile strain | Break | ISO 527-2 | >50 % |
| Bending modulus | ISO 178 | 900 Mpa | |
| Tensile modulus | ISO 527-2 | 900 Mpa | |
| thermal performance | Test Condition | Test Method | DUPONT USA/FN727 |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 55.0 °C |
| Glass transition temperature | ISO 11357-2 | 55.0 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 48.0 °C |
| Melting temperature | ISO 11357-3 | 221 °C | |
| flammability | Test Condition | Test Method | DUPONT USA/FN727 |
| Burning rate | 1.00mm | ISO 3795 | <100 mm/min |
| FMVSS flammability | FMVSS302 | B |