PA6 FN727 DUPONT USA
Zytel®
Electronic and electrical、Automotive Applications
Thermal stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | DUPONT USA/FN727 |
---|---|---|---|
Tensile modulus | ISO 527-2 | 900 Mpa | |
Tensile strain | 断裂 | ISO 527-2 | >50 % |
Flexural modulus | ISO 178 | 900 Mpa | |
tensile strength | 50%应变 | ISO 527-2 | 28.0 Mpa |
flammability | Test Condition | Test Method | DUPONT USA/FN727 |
---|---|---|---|
FMVSS flammability | FMVSS302 | B | |
burning rate | 1.00mm | ISO 3795 | <100 mm/min |
physical property | Test Condition | Test Method | DUPONT USA/FN727 |
---|---|---|---|
Shrinkage rate | TD | ISO 294-4 | 1.2 % |
MD | ISO 294-4 | 0.80 % | |
MediumDensity | 0.870 g/cm³ | ||
SpecificHeatCapacity of Melt | 2700 J/kg/°C | ||
ThermalConductivityofMelt | 0.16 W/m/K | ||
Water absorption rate | 平衡,23°C,2.00mm,50%RH | ISO 62 | 1.4 % |
Thermal performance | Test Condition | Test Method | DUPONT USA/FN727 |
---|---|---|---|
melting temperature | ISO 11357-3 | 221 °C | |
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 55.0 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 48.0 °C | |
Glass Transition Temperature | ISO 11357-2 | 55.0 °C |