Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PBI (T Series) TL-60 PBI USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodPBI USA/ (T Series) TL-60
Rockwell hardnessA计秤ASTM D78524
Supplementary InformationTest ConditionTest MethodPBI USA/ (T Series) TL-60
Initial weightlessness temperatureNitrogen内部方法606 °C
Air内部方法602 °C
Mechanical propertiesTest ConditionTest MethodPBI USA/ (T Series) TL-60
coefficient of friction与钢-动态0.050
elongation断裂ASTM D6380.90 %
tensile strength ASTM D638110 MPa
compressive strengthASTM D695124 MPa
Tensile modulusASTM D63817900 MPa
Flexural modulusASTM D79013100 MPa
Compression ModulusASTM D6955100 MPa
coefficient of friction与钢-静态0.30
WearRate0.200 in/1000hr
bending strengthASTM D790159 MPa
Poisson's ratio0.42
physical property Test ConditionTest MethodPBI USA/ (T Series) TL-60
density1.43 g/cm³
Water absorption rate平衡ASTM D5703.8 %
23°C,24hrASTM D5700.20 %
Thermal performanceTest ConditionTest MethodPBI USA/ (T Series) TL-60
Heat distortion temperature1.8MPa,未退火,HDTASTM D648310 °C
HeatCapacity70°CDSC1170 J/kg/°C
Linear coefficient of thermal expansionMD:24到149°CTMA2.5E-05 cm/cm/°C
Running177 °C
thermal conductivity21°CASTMF4330.76 W/m/K

Contact Us

Get App

Top