Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | SABIC SAUDI/71EK71PS |
|---|---|---|---|
| Impact strength of cantilever beam gap | 0℃ | ISO 180/4A | 9.0 KJ/m |
| Charpy Notched Impact Strength | -20℃ | ISO 179 | 7.2 KJ/m |
| elongation | Break | ISO 527 | 500 % |
| Impact strength of cantilever beam gap | -20℃ | ISO 180/4A | 5.0 KJ/m |
| tensile strength | Yield | ISO 527 | 35 Mpa |
| Bending modulus | ASTM D-790 | 1500 Mpa | |
| Charpy Notched Impact Strength | 23℃ | ISO 179 | 70 KJ/m |
| tensile strength | Break | ISO 527 | 39 Mpa |
| thermal performance | Test Condition | Test Method | SABIC SAUDI/71EK71PS |
| Hot deformation temperature | 0.45MPa (HDT/B) | ISO 75/B | 94 °C |
| Vicat softening temperature | 10N (VST/A) | ISO 306/A | 155 °C |
| Basic Performance | Test Condition | Test Method | SABIC SAUDI/71EK71PS |
| melt mass-flow rate | 230℃,2.16kg | ISO 1133 | 0.30 g/10min |
| density | ISO 1183 | 0.905 |