thermal performanceTest ConditionTest MethodKUMHO KOREA/HAG5220
Hot deformation temperature1.80MPa,UnannealedASTM D-648100 °C
CombustibilityUL 94HB
Vicat softening temperatureASTM D-1525115 °C
mechanical propertiesTest ConditionTest MethodKUMHO KOREA/HAG5220
Rockwell hardnessASTM D-785108 R scale
Impact strength of cantilever beam gap23℃,3.20mmASTM D-25690.7 J/m
elongation at yield23℃ASTM D-6387.0 %
tensile strengthYield,23℃ASTM D-63878.4 Mpa
bending strength23℃,YieldASTM D-790108 Mpa
Impact strength of cantilever beam gap23℃,6.40mmASTM D-25680.1 J/m
Bending modulus23℃ASTM D-7903920 Mpa
Basic PerformanceTest ConditionTest MethodKUMHO KOREA/HAG5220
melt mass-flow rate230℃,21.6kgASTM D-123880 g/10min
Physical propertiesTest ConditionTest MethodKUMHO KOREA/HAG5220
Shrinkage rateFlowASTM D-9550.10-0.30 %