Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC L-1250Z100 TEIJIN SINGAPORE
PANLITE®
Electrical applications,Casters
Weather resistance,standard
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | TEIJIN SINGAPORE/L-1250Z100 |
|---|---|---|---|
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 142 °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 129 °C | |
| Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 7.0E-5 cm/cm/°C |
| Flow | ISO 11359-2 | 7.0E-5 cm/cm/°C | |
| RTI | 0.75 mm | UL 746 | 125 °C |
| RTI Elec | 0.75 mm | UL 746 | 125 °C |
| RTI Imp | 0.75 mm | UL 746 | 115 °C |
| Vicat softening temperature | ISO 306/B50 | 149 °C |
| mechanical properties | Test Condition | Test Method | TEIJIN SINGAPORE/L-1250Z100 |
|---|---|---|---|
| Bending modulus | ISO 178 | 2350 Mpa | |
| bending strength | ISO 178 | 93.0 Mpa | |
| Nominal tensile fracture strain | ISO 527-2/50 | > 50 % | |
| Tensile modulus | ISO 527-2/1 | 2400 Mpa | |
| Tensile strain | Yield | ISO 527-2/50 | 6.0 % |
| tensile strength | Yield | ISO 527-2/50 | 61.0 Mpa |
| Electrical performance | Test Condition | Test Method | TEIJIN SINGAPORE/L-1250Z100 |
|---|---|---|---|
| Compared to the anti leakage trace index | IEC 60112 | PLC 2 | |
| Dielectric strength | IEC 60243-1 | 30 KV/mm | |
| Dissipation factor | 100 Hz | IEC 60250 | 1.0E-3 |
| 1 MHz | IEC 60250 | 9.0E-3 | |
| Relative permittivity | 100 Hz | IEC 60250 | 3.10 |
| 1 MHz | IEC 60250 | 3.00 | |
| Surface resistivity | IEC 60093 | > 1.0E+15 ohms | |
| Volume resistivity | IEC 60093 | > 1.0E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | TEIJIN SINGAPORE/L-1250Z100 |
|---|---|---|---|
| density | ISO 1183 | 1.20 g/cm³ | |
| Melt Volume Flow Rate (MVR) | 300°C/1.2 kg | ISO 1133 | 8.00 cm3/10min |
| Shrinkage rate | Flow : 4.00 mm | Internal Method | 0.50 - 0.70 % |
| 横向Flow : 4.00 mm | Internal Method | 0.50 - 0.70 % | |
| Water absorption rate | 24 hr, 23°C | ISO 62 | 0.20 % |
| impact performance | Test Condition | Test Method | TEIJIN SINGAPORE/L-1250Z100 |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | 76 kJ/m² | |
| Impact strength of simply supported beam without notch | ISO 179 | 无断裂 |
| flammability | Test Condition | Test Method | TEIJIN SINGAPORE/L-1250Z100 |
|---|---|---|---|
| Burning wire flammability index | 3.0 mm | IEC 60695-2-12 | 875 °C |
| 1.5 mm | IEC 60695-2-12 | 825 °C | |
| Hot filament ignition temperature | 1.5 mm | IEC 60695-2-13 | 850 °C |
| 3.0 mm | IEC 60695-2-13 | 850 °C | |
| UL flame retardant rating | 0.40 mm | UL 94 | V-2 |
| 1.5 mm | UL 94 | HB |
| optical performance | Test Condition | Test Method | TEIJIN SINGAPORE/L-1250Z100 |
|---|---|---|---|
| Refractive index | ASTM D542 | 1.585 | |
| transmissivity | 3000 μm | ASTM D1003 | 88.0 % |