Rubber Shin-Etsu Elastomer SV-55002U Shin-Etsu Silicones of America
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer SV-55002U |
---|---|---|---|
Shore hardness | 50 |
Supplementary Information | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer SV-55002U |
---|---|---|---|
CureAgent | DBPH |
thermosetting | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer SV-55002U |
---|---|---|---|
Post curing time | 200°C | 4.0 hr |
Uncured Properties | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer SV-55002U |
---|---|---|---|
Curing Time | 0.17 hr |
physical property | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer SV-55002U |
---|---|---|---|
density | 1.13 g/cm³ |
elastomer | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer SV-55002U |
---|---|---|---|
tear strength | 33.3 kN/m | ||
elongation | 断裂 | 660 % | |
tensile strength | 9.31 MPa | ||
compression set | 100°C,70hr | 10 % |