Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPEE HTR8685 BK DUPONT USA
Hytrel®
Automotive Applications,Cable,Blow molding applications
High temperature resistan,Chemical resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | DUPONT USA/HTR8685 BK |
|---|---|---|---|
| Shore hardness | ShoreD | ISO 868 | 44 |
| ShoreD,15Sec | ISO 868 | 41 |
| thermal performance | Test Condition | Test Method | DUPONT USA/HTR8685 BK |
|---|---|---|---|
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 2E-04 cm/cm/°C |
| MD | ISO 11359-2 | 2.1E-04 cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 206 °C |
| mechanical properties | Test Condition | Test Method | DUPONT USA/HTR8685 BK |
|---|---|---|---|
| Bending modulus | ISO 178 | 100 Mpa | |
| Nominal tensile fracture strain | ISO 527-2 | 350 % | |
| Tensile modulus | ISO 527-2 | 100 Mpa | |
| Tensile strain | Break | ISO 527-2 | >300 % |
| tensile strength | 50%Strain | ISO 527-2 | 14.0 Mpa |
| 10%Strain | ISO 527-2 | 8.40 Mpa | |
| Break | ISO 527-2 | 30.0 Mpa |
| Physical properties | Test Condition | Test Method | DUPONT USA/HTR8685 BK |
|---|---|---|---|
| Shrinkage rate | MD | ISO 294-4 | 1.7 % |
| TD | ISO 294-4 | 1.6 % |
| flammability | Test Condition | Test Method | DUPONT USA/HTR8685 BK |
|---|---|---|---|
| Burning rate | 1.00mm | ISO 3795 | <100 mm/min |
| FMVSS flammability | FMVSS302 | B |
| elastomer | Test Condition | Test Method | DUPONT USA/HTR8685 BK |
|---|---|---|---|
| tear strength | 横向Flow | ISO 34-1 | 110 kN/m |
| Flow | ISO 34-1 | 110 kN/m |