Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC/ABS SK2706N 1535T IDEMITSU JAPAN
TARFLON™
Automotive Applications,Electronic and electrical components
Medium viscosity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | IDEMITSU JAPAN/SK2706N 1535T |
|---|---|---|---|
| ISO Shortcut | >PC+ABS-FR(40)< |
| thermal performance | Test Condition | Test Method | IDEMITSU JAPAN/SK2706N 1535T |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 88.0 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 78.0 °C | |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 5.8E-05 cm/cm/°C |
| RTI Elec | UL 746 | 60.0 °C | |
| RTI Imp | UL 746 | 60.0 °C | |
| RTI Str | UL 746 | 60.0 °C |
| mechanical properties | Test Condition | Test Method | IDEMITSU JAPAN/SK2706N 1535T |
|---|---|---|---|
| Bending modulus | ISO 178 | 3000 Mpa | |
| bending strength | ISO 178 | 90.0 Mpa | |
| Nominal tensile fracture strain | ISO 527-2 | 50 % | |
| tensile strength | Yield | ISO 527-2 | 64.0 Mpa |
| Electrical performance | Test Condition | Test Method | IDEMITSU JAPAN/SK2706N 1535T |
|---|---|---|---|
| Dielectric strength | IEC 60243-1 | 36 KV/mm |
| Physical properties | Test Condition | Test Method | IDEMITSU JAPAN/SK2706N 1535T |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 260°C/2.16kg | ISO 1133 | 20.0 cm3/10min |
| Shrinkage rate | MD:2.00mm | Internal Method | 0.40 % |
| TD:2.00mm | Internal Method | 0.40 % | |
| Spiral flow length | Internal Method | 40.0 CM | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.10 % |
| flammability | Test Condition | Test Method | IDEMITSU JAPAN/SK2706N 1535T |
|---|---|---|---|
| UL flame retardant rating | 0.58mm | UL 94 | V-1 |
| 1.0mm | UL 94 | V-0 | |
| 0.8mm | UL 94 | 5VB |