Thermal Properties | Test Condition | Test Method | SABIC INNOVATIVE US/D351-8R9D107 |
---|---|---|---|
Coefficient of Linear Thermal Expansion | MD | ASTMD696 | 2E-05 cm/cm/°C |
Heat Deflection Temperature | 1.80MPa未退火 | ASTMD648 | 116 °C |
Coefficient of Linear Thermal Expansion | TD | ASTMD696 | 6.7E-05 cm/cm/°C |
Physical | Test Condition | Test Method | SABIC INNOVATIVE US/D351-8R9D107 |
---|---|---|---|
Modeling Shrinkage | TD | ASTMD995 | 0.3 % |
MD | ASTMD995 | 0.1 % | |
Melt Mass-Flow Rate | 300℃/2.16Kg | ASTMD1238 | 25 g/10min |
Mechanical Properties | Test Condition | Test Method | SABIC INNOVATIVE US/D351-8R9D107 |
---|---|---|---|
Flexural Strength | 23°C | ASTMD790 | 179 Mpa |
Flexural Modulus | 23°C | ASTMD790 | 8400 Mpa |
Notched Izod Impact Strength | 23°C | ASTMD256 | 150 J/m |
Unnotched Izod Impact Strength | 23°C | ASTMD256 | 510 J/m |
Tensile Strength | 23°C | ASTMD638 | 120 Mpa |
Tensile Modulus | 23°C | ASTMD638 | 9050 Mpa |
Tensile Elongation?(Break) | 23°C | ASTMD638 | 2 % |
Flammability | Test Condition | Test Method | SABIC INNOVATIVE US/D351-8R9D107 |
---|---|---|---|
Fire rating | UL-94 | 0.8mm V-0 |