PP 6936G2 EXXONMOBIL USA
--
Melt blown non-woven fabr、Personal care、Industrial applications、Filter material、Medical/nursing supplies、Filter material
High mobility
TDS
TDS
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | EXXONMOBIL USA/6936G2 |
---|---|---|---|
Impact strength of simply supported beam without notch | 23℃ | kJ/m² | 2.229to8.821 |
Dart impact | 23℃ | N.m | 26.55to73.89 |
hardness | Test Condition | Test Method | EXXONMOBIL USA/6936G2 |
---|---|---|---|
ball-indentation hardness | 74.48to85.52 MPa | ||
Rockwell hardness | 23℃ | 84to106 |
Mechanical properties | Test Condition | Test Method | EXXONMOBIL USA/6936G2 |
---|---|---|---|
Yield, 23 ℃ | 51.38to55.59 MPa | ||
% | 2.6to7.2 | ||
Fracture, 23 ℃ | 19.03to32.83 MPa | ||
% | 2.0to31 |
Electrical performance | Test Condition | Test Method | EXXONMOBIL USA/6936G2 |
---|---|---|---|
Surface Resistivity | ohms | 1.0E+14-1.0E+15 | |
Compared to the Leakage Tracking Index (CTI) | V |
optical performance | Test Condition | Test Method | EXXONMOBIL USA/6936G2 |
---|---|---|---|
gloss | 46to47 |
flammability | Test Condition | Test Method | EXXONMOBIL USA/6936G2 |
---|---|---|---|
Limiting Oxygen Index | % | 21 | |
burning rate | mm/min | 0.0to101.6 | |
Hot filament ignition temperature | °C | 548to804 | |
Burning wire flammability index | °C | 643to960 |
physical property | Test Condition | Test Method | EXXONMOBIL USA/6936G2 |
---|---|---|---|
230°C/2.16kg | g/10min | 4.9to21 | |
Flow: 23 ℃ | 流动,23℃ | mm/mm | 139.7E-3-0.432 |
Melt volume flow rate | 230°C/2.16kg | ISO 527-2/5 | 0.01to0.07 |
23℃,24hr | % | 0.020to0.052 | |
Lateral flow: 23 ℃ | 横向, 23℃ | mm/mm | 0.279to0.457 |
Thermal performance | Test Condition | Test Method | EXXONMOBIL USA/6936G2 |
---|---|---|---|
0.45MPa, Not annealed | °C | 110to139 | |
1.8MPa, Not annealed | °C | 58to91 |