Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Reference Price
| Physical properties | Test Condition | Test Method | SK KOREA/T110-PRO |
|---|---|---|---|
| Water absorption rate | Equilibrium | ASTM D570 | 0.20to0.30 % |
| Shrinkage rate | MD | ASTM D955 | 0.20-0.30 % |
| mechanical properties | Test Condition | Test Method | SK KOREA/T110-PRO |
| elongation | Break | ASTM D638 | 150 % |
| tensile strength | Break | ASTM D638 | 44.0 Mpa |
| Yield | ASTM D638 | 51.0 Mpa | |
| Bending modulus | ASTM D790 | 2180 Mpa | |
| elongation | Yield | ASTM D638 | 6.8 % |
| bending strength | ASTM D790 | 86.0 Mpa | |
| thermal performance | Test Condition | Test Method | SK KOREA/T110-PRO |
| Glass transition temperature | ASTME1356 | 110 °C | |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 100 °C |
| optical performance | Test Condition | Test Method | SK KOREA/T110-PRO |
| turbidity | ASTM D1003 | <1.0 % | |
| Refractive index | ASTM D542 | 1.560 | |
| transmissivity | ASTM D1003 | 89.0 % | |
| hardness | Test Condition | Test Method | SK KOREA/T110-PRO |
| Rockwell hardness | R-Scale | ASTM D785 | 119 |