PEK LUVOCOM® 1104-7452 VP LEHVOSS Group
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | LEHVOSS Group/LUVOCOM® 1104-7452 VP |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.0 kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1fU | 45 kJ/m² |
Mechanical properties | Test Condition | Test Method | LEHVOSS Group/LUVOCOM® 1104-7452 VP |
---|---|---|---|
Tensile modulus | ISO 527-2 | 11500 MPa | |
tensile strength | 断裂 | ISO 527-2 | 180 MPa |
Tensile strain | 屈服 | ISO 527-2 | 2.1 % |
Bending Strain | ISO 178 | 2.7 % | |
Flexural modulus | ISO 178 | 9000 MPa | |
bending strength | ISO 178 | 260 MPa |
Electrical performance | Test Condition | Test Method | LEHVOSS Group/LUVOCOM® 1104-7452 VP |
---|---|---|---|
insulation resistance | IEC 60167 | >1.0E+12 ohms |
physical property | Test Condition | Test Method | LEHVOSS Group/LUVOCOM® 1104-7452 VP |
---|---|---|---|
Shrinkage rate | DIN 16901 | 0.30to0.60 % | |
Water absorption rate | 23°C,24hr | <0.10 % | |
density | ISO 1183 | 1.53 g/cm³ |
Thermal performance | Test Condition | Test Method | LEHVOSS Group/LUVOCOM® 1104-7452 VP |
---|---|---|---|
thermal conductivity | DIN 52612 | 0.40 W/m/K | |
Continuous use temperature | UL 746B | 260 °C | |
vicat | ISO 306/A | 325 °C | |
Linear coefficient of thermal expansion | MD | DIN 53752 | 2.2E-05 cm/cm/°C |
maximum service temperature | ShortTerm | 290 °C |