Basic performance | Test Condition | Test Method | Schulman Plastics/WR/MI-E |
---|---|---|---|
Water absorption rate | ISO 62 | 1.2 % | |
density | ISO 1183 | 1060 kg/m | |
Melt volume flow rate | 220℃,10kg | ISO 1133 | 11.0 cm |
Electrical performance | Test Condition | Test Method | Schulman Plastics/WR/MI-E |
---|---|---|---|
Dielectric loss | 1MHz | IEC 60250 | 0.0090 |
relative permittivity | 100Hz | IEC 60250 | 3.20 |
Dielectric loss | 100Hz | IEC 60250 | 0.012 |
Volume resistivity | IEC 60093 | >1.0E+13 ohm.m | |
relative permittivity | 1MHz | IEC 60250 | 3.00 |
Surface Resistivity | IEC 60093 | >1.0E+15 ohms |
Mechanical properties | Test Condition | Test Method | Schulman Plastics/WR/MI-E |
---|---|---|---|
Tensile strain | 屈服 | ISO 527-1 | 3.5 % |
Tensile modulus | ISO 527-1 | 2200 MPa | |
Tensile stress | 屈服 | ISO 527-1 | 46.0 MPa |
Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 11.0 KJ/m |
fracture strain | ISO 527-1 | 37.0 % |
Thermal performance | Test Condition | Test Method | Schulman Plastics/WR/MI-E |
---|---|---|---|
vicat | 50℃/h 50N | ISO 306 | 102 ℃ |
Linear coefficient of thermal expansion | normal | ISO 11359-1 | 0.000090 cm/cm℃ |
Heat distortion temperature | 1.80MPa,HDT | ISO 75-1 | 87.0 |
Linear coefficient of thermal expansion | parallel | ISO 11359-1 | 0.000090 cm/cm℃ |
Heat distortion temperature | 0.45MPa,HDT | ISO 75-1 | 104 ℃ |