Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP Homopolymer TOLEN H030 GP/3 SIBUR RUSSIA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | SIBUR RUSSIA/TOLEN H030 GP/3 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ISO 180 | 2.0 kJ/m² |
Mechanical properties | Test Condition | Test Method | SIBUR RUSSIA/TOLEN H030 GP/3 |
---|---|---|---|
Flexural modulus | ISO 178 | 1400 MPa | |
Tensile strain | 屈服 | ISO 527-2/50 | 10 % |
tensile strength | 屈服 | ISO 527-2/50 | 34.0 MPa |
physical property | Test Condition | Test Method | SIBUR RUSSIA/TOLEN H030 GP/3 |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 3.0 g/10min |
Thermal performance | Test Condition | Test Method | SIBUR RUSSIA/TOLEN H030 GP/3 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 80.0 °C |
vicat | ISO 306/A | 155 °C |