Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPS R-7-120 BL CPCHEM SINGAPHORE
RYTON®
Automotive sector,Electronic communication accessories,Electronic communication accessories,Application in the automotive field
Flame retardant,High rigidity,wear resistant,Chemical resistance,High temperature resistan,Filler: Glass mineral,Filler: Glass mineral
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | CPCHEM SINGAPHORE/R-7-120 BL |
---|---|---|---|
Rockwell hardness | M-Sale | ASTM D785 | 101 |
R-Sale | ASTM D785 | 118 |
thermal performance | Test Condition | Test Method | CPCHEM SINGAPHORE/R-7-120 BL |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 265 °C |
Linear coefficient of thermal expansion | MD:100to200°C | ASTME831 | 1.5E-05 cm/cm/°C |
MD:-50to50°C | ASTME831 | 1.5E-05 cm/cm/°C | |
TD:-50to50°C | ASTME831 | 3E-05 cm/cm/°C | |
TD:导热系数 | ASTME831 | 0.59 W/m/K | |
TD:100to200°C | ASTME831 | 7E-05 cm/cm/°C | |
UL temperature rating | UL 746B | 220to240 °C |
mechanical properties | Test Condition | Test Method | CPCHEM SINGAPHORE/R-7-120 BL |
---|---|---|---|
Bending modulus | ISO 178 | 19000 Mpa | |
ASTM D790 | 19300 Mpa | ||
bending strength | ASTM D790 | 207 Mpa | |
ISO 178 | 210 Mpa | ||
compressive strength | ASTM D695 | 265 Mpa | |
elongation | Break | ASTM D638 | 0.90 % |
Poisson's ratio | ISO 527 | 0.36 | |
Tensile strain | Break | ISO 527-2 | 0.80 % |
tensile strength | ASTM D638 | 124 Mpa | |
ISO 527-2 | 135 Mpa |
Electrical performance | Test Condition | Test Method | CPCHEM SINGAPHORE/R-7-120 BL |
---|---|---|---|
Arc resistance | ASTM D495 | 185 sec | |
Compared to the anti leakage trace index | CTI | UL 746 | PLC 2 |
Dielectric constant | 25°C,1kHz | ASTM D150 | 4.90 |
25°C,1MHz | ASTM D150 | 4.90 | |
Dielectric strength | ASTM D149 | 16 KV/mm | |
Dissipation factor | 25°C,1kHz | ASTM D150 | 4E-03 |
25°C,1MHz | ASTM D150 | 2E-03 | |
insulation resistance | 90°C | 1E+11 ohms | |
Surface resistivity | ASTM D257 | 1E+16 ohms | |
Volume resistivity | ASTM D257 | 1E+15 ohms·cm |
Physical properties | Test Condition | Test Method | CPCHEM SINGAPHORE/R-7-120 BL |
---|---|---|---|
density | ASTM D792 | 1.99 g/cm³ | |
Shrinkage rate | MD:3.20mm | 0.20 % | |
TD:3.20mm | 0.40 % | ||
Water absorption rate | 23°C,24hr | ASTM D570 | 0.020 % |
impact performance | Test Condition | Test Method | CPCHEM SINGAPHORE/R-7-120 BL |
---|---|---|---|
Impact strength of cantilever beam gap | ISO 180/A | 6.0 kJ/m² | |
3.17mm | ASTM D256 | 53 J/m | |
Suspended wall beam without notch impact strength | ISO 180 | 15 kJ/m² | |
3.18mm | ASTM D4812 | 210 J/m |
flammability | Test Condition | Test Method | CPCHEM SINGAPHORE/R-7-120 BL |
---|---|---|---|
Extreme Oxygen Index | ASTM D2863 | 61 % | |
UL flame retardant rating | 1.6mm | UL 94 | V-05VA |