Material Comparison
Add Comparison Model
Highlight Differences
Hide Same

Product Name / Manufacturer / Model

Brand

Typical Applications

Properties

Color

Form

Processing Methods

Grade

Filler

Recycled Content

Certificates

Reference Price

thermal performanceTest ConditionTest MethodTORAY MALAYSIA/100G-30 BK
Hot deformation temperature1.82MpaASTM D-648104 °C
Ball indentation temperature95 °C
UL flame retardant ratingUL 94HB
mechanical propertiesTest ConditionTest MethodTORAY MALAYSIA/100G-30 BK
Rockwell hardness23℃ 50RHASTM D-785125 R-Scale
Impact strength of cantilever beam gap23℃ 12.7mmASTM D-25649 J/m
elongationBreakASTM D-6383 %
Bending modulus23℃ 50RHASTM D-7908500 Mpa
tensile strength23℃ 50RHASTM D-638118 Mpa
bending strength23℃ 50RHASTM D-790160 Mpa
Basic PerformanceTest ConditionTest MethodTORAY MALAYSIA/100G-30 BK
melt mass-flow rate220℃/98NISO 11338 g/10min
Physical propertiesTest ConditionTest MethodTORAY MALAYSIA/100G-30 BK
Shrinkage rate0.1-0.3 %

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China