EVA UE630 USI TAIWAN
EVATHENE®
Compression molding (foaming) coating, extrusion b
--
MSDS
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | USI TAIWAN/UE630 |
---|---|---|---|
Vinyl acetate content | USIFE | 16 % |
Basic Performance | Test Condition | Test Method | USI TAIWAN/UE630 |
---|---|---|---|
density | ASTM D-1505 | 0.937 g/cm³ | |
melt mass-flow rate | ASTM D-1238 | 1.5 g/10min |
thermal performance | Test Condition | Test Method | USI TAIWAN/UE630 |
---|---|---|---|
Melting temperature | ASTM D-2117 | 89 °C | |
Vicat softening temperature | ASTM D-1525 | 67 °C |
mechanical properties | Test Condition | Test Method | USI TAIWAN/UE630 |
---|---|---|---|
elongation | 射出 | ASTM D-638(ASTM D-882) | 150 % |
薄膜TD | ASTM D-638(ASTM D-882) | 670 % | |
铸膜成型 | ASTM D-638(ASTM D-882) | 700 % | |
薄膜MD | ASTM D-638(ASTM D-882) | 310 % | |
Impact strength of cantilever beam gap | ASTM D-1709 | 430 G/F50 | |
Low temperature brittleness temperature | ASTM D-746 | <-76 ℃/F50 | |
Shore hardness | ASTM D-2240 | 36 Shore D | |
tensile strength | 铸膜成型,Yield | ASTM D-638(ASTM D-882) | 170 kg/cm2 |
薄膜TD,Yield | ASTM D-638(ASTM D-882) | 184 kg/cm2 | |
薄膜MD,Yield | ASTM D-638(ASTM D-882) | 213 kg/cm2 | |