| Physical properties | Test Condition | Test Method | STYRON US/3002 |
|---|---|---|---|
| Content of comonomer | Internal Method | 8.0 % | |
| melt mass-flow rate | 190°C/2.16kg | ASTMD1238 | 9.8 g/10min |
| mechanical properties | Test Condition | Test Method | STYRON US/3002 |
| Tensile modulus | 2%Secant | ASTMD638 | 110 Mpa |
| elongation | Break | ASTMD638 | 570 % |
| tensile strength | Yield | ASTMD638 | 7.00 Mpa |
| Break | ASTMD638 | 19.0 Mpa | |
| thermal performance | Test Condition | Test Method | STYRON US/3002 |
| Melting temperature | Internal Method | 100 °C | |
| Vicat softening temperature | -- | ISO 306 | 82.0 °C |
| -- | ASTM D1525 | 82.2 °C | |
| film | Test Condition | Test Method | STYRON US/3002 |
| Water vapor permeability | 38°C,90%RH | DIN 53122/2 | 0.40 g·mm/m²/atm/24hr |
| Initial sealing temperature | Internal Method | 85.0 °C | |
| hardness | Test Condition | Test Method | STYRON US/3002 |
| Shore hardness | ShoreD | ASTMD2240 | 53 |