Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PBT SF3300 ED3002 JAPAN POLYPLASTIC
--
--
Filler: Glass fiber reinf,30% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | JAPAN POLYPLASTIC/SF3300 ED3002 |
|---|---|---|---|
| ColourNumber | ED3002 |
| thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/SF3300 ED3002 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 213 °C |
| mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/SF3300 ED3002 |
|---|---|---|---|
| Bending modulus | ISO 178 | 9340 Mpa | |
| bending strength | ISO 178 | 218 Mpa | |
| Tensile strain | Break | ISO 527-2 | 1.9 % |
| tensile strength | ISO 527-2 | 135 Mpa |
| flammability | Test Condition | Test Method | JAPAN POLYPLASTIC/SF3300 ED3002 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |